PP is a semi-crystalline polymer. Its melting temperature (Tm) is 160–170 °C, its glass transition temperature (Tg) is −10 °C and its density is 0.90–0.91 g/cm³. In the typical injection reference, melt temperature is 200–280 °C and mold temperature is 30–80 °C.
- Warpage tendency: In a semi-crystalline structure, some pigments act like nucleating agents and can increase shrinkage and warpage. For parts with a warpage risk, pigments with a low nucleating effect are selected.
- Migration: Pigment migration risk is low in polyolefins (PE/PP); grade 4–5 on the gray scale.
- Thermal degradation: Under high temperature and shear, PP undergoes chain scission, which shows up as an MFI increase and embrittlement.
- UV degradation: In outdoor PP products, UV radiation causes color loss, cracking and chalking.
Recommended Colorex Masterbatches and Additives
- Color masterbatch: Produced with a compatible carrier for PP homopolymer and copolymer; used at 1.5–3.0% in injection and blow molding and at 2.0–4.0% in thin film and fiber.
- White masterbatch: Provides high opacity with rutile TiO₂; 1.5–4.0% is recommended in standard injection and 2.5–6.0% in thin-wall IML.
- Black masterbatch: Delivers high opacity at 1.5–3.0% in general injection, crates and pallets.
- Transparent masterbatch: Works with nucleating (clarifier) additives in random copolymer PP to give colored transparent parts with low haze.
- UV & light stabilizer: Protects outdoor products such as garden furniture and raffia; used at 1.0–3.0% in thick injection parts and 2.0–6.0% in thin film and raffia.
- Antioxidant masterbatch: Limits MFI increase and yellowing on raffia, pipe and recycling lines running at high temperature; general dosage 0.5–2.0%.
- Filler masterbatch: Used at 5.0–25.0% in PP raffia and sack tapes to increase stiffness and reduce raw material cost.
- Slip masterbatch: Balances opening torque in PP closures and eases part release from the mold; 1.5–2.5% in caps and closures.
Notes by Process
- Injection molding: A color masterbatch dosage of 1.5–3.0% is sufficient for most parts. Plants that create their own color at the machine with a gravimetric doser can use mono masterbatch.
- Raffia and tape: The typical color masterbatch dosage is 1–3%. Since agglomerated pigment leads to tape breaks, a product with a low filter pressure value (FPV) should be selected. In calcite-filled recipes, desiccant masterbatch prevents moisture-related tape breaks.
- Film (CPP, BOPP): Slip is used to lower friction and antiblock masterbatch to keep layers from sticking; both additives can be combined in a single granule.
- Transparent PP: Transparent masterbatch is used at 0.3–1.0% for light pastel transparent shades and 1.0–2.5% for vivid, deep shades.
Points to Watch
- The carrier resin should be selected according to the melt flow (MFI) of the base polymer; an incompatible carrier causes phase separation and loss of mechanical properties.
- PE and PP have limited compatibility; if a product with a different carrier is used, its mechanical effect should be checked in the laboratory.
- Pigment heat resistance should be evaluated together with the process temperature. For example, diarylide yellow (PY83) and diarylide orange (PO34) have a heat resistance of 200–230 °C, which is below PP's upper processing temperatures.
- Pigments with high lightfastness should be selected for outdoor products; diarylide yellow, with a lightfastness of 3–4, is suitable for indoor use only.
Frequently Asked Questions
At what ratio is color masterbatch used in PP?
Colorex color masterbatches are used at 1.5–3.0% in injection, blow molding and pipe/profile applications, and at 2.0–4.0% in thin film and fiber. The exact ratio depends on shade depth, opacity target and part thickness.
What should be considered in masterbatch selection to prevent warpage in PP parts?
Since PP is a semi-crystalline polymer, some pigments can affect crystallization and cause different shrinkage in different directions, leading to warpage. For parts with this risk, pigments with a low nucleating effect are preferred.
How are PP products used outdoors protected?
UV and light stabilizers are used in garden furniture, raffia and similar products. A dosage of 1.0–3.0% is recommended for thick injection parts and 2.0–6.0% for thin film and raffia; the package is selected according to product thickness and the solar radiation of the region of use.