Properties Relevant to Coloring and Additives
PET is a semi-crystalline polymer. Its melting temperature (Tm) is 250–260 °C, its glass transition temperature (Tg) is 70–80 °C and its density is 1.38–1.40 g/cm³. In the typical injection reference, melt temperature is 260–280 °C and mold temperature is 20–30 °C.
- Moisture sensitivity: PET absorbs moisture and must be dried before production; otherwise moisture lowers the molecular weight through hydrolysis.
- High processing temperature: Pigments and additives must not lose color or degrade at these temperatures.
- Migration: Migration risk is low in engineering plastics such as PA, PC and PET; grade 4–5 on the gray scale.
- Crystallization and haze: If an unsuitable pigment is selected, haze increases in PET trays; a masterbatch that does not disturb crystallization is preferred.
Recommended Colorex Masterbatches and Additives
- Transparent masterbatch: Preserves transparency in bottles and containers with polymer-soluble dyes and nano-dispersed organic pigments; the target light transmission is above 88%. Used at 0.3–1.0% for pastel shades and 1.0–2.5% for vivid shades.
- Mono masterbatch: Single pigment concentrates with a PET carrier suit plants that create their own color at the machine and fiber lines; generally 0.2–3.0%.
- Color masterbatch: For opaque colors, a dedicated series is prepared after carrier compatibility with PET is verified in the laboratory.
- Desiccant masterbatch: Binds free moisture remaining in the melt and acts as a complementary safeguard to pre-drying; in PET it does not replace drying.
- Odor eliminating masterbatch: Acetaldehyde-scavenging solutions are offered against acetaldehyde-related odor and taste transfer in rPET; dosage 1.0–3.0%.
- Compatibilizer and chain extender: Reduces the brittleness of rPET whose chains are shortened during recycling and makes the PP/PE mixture from caps and labels compatible.
- Antistatic masterbatch: In PET, heat-resistant or permanent systems are preferred over standard migratory agents.
Notes by Process
- Blow molding (bottles and containers): Transparent masterbatch is used for transparent shades. For opaque bottles, the general reference dosage for color masterbatch is 2–5%; opacity and gloss are targeted together.
- Trays and sheet: Pigments and masterbatches that do not disturb crystallization are selected to prevent increased haze.
- Fiber and yarn: A PET-based carrier should be used for polyester. In yarn spinning, pigment particles must be dispersed below 1 μm and the FPV must be below 1.0 bar/g; otherwise screen pressure rises and the yarn breaks.
- rPET fiber: The variable yellowish tone of rPET is brought to a neutral base with a masterbatch containing toner or bluing agent before the target color is built.
Points to Watch
- PET and the masterbatch granules should be dried before processing; a desiccant additive only complements drying.
- Pigment heat resistance should be above the melt temperature (260–280 °C). Titanium dioxide, carbon black and iron oxide red have a heat resistance above 300 °C and phthalocyanine blue and green 280–300 °C; diarylide yellow and orange (200–230 °C) and iron oxide yellow (180–200 °C) are insufficient for these temperatures.
- In transparent applications, the carrier resin must also be clear and match the refractive index of the base polymer; otherwise haze may increase.
Frequently Asked Questions
Is drying required before using masterbatch in PET?
Yes. PET is a hygroscopic polymer, and moisture lowers its molecular weight through hydrolysis. Desiccant masterbatch provides support by binding free moisture in the melt, but it does not replace standard pre-drying.
How is transparent color achieved in PET bottles?
Transparent masterbatches use polymer-soluble dyes and very finely dispersed organic pigments with a matching refractive index, so light is not scattered and light transmission is kept above 88%. Dosage is 0.3–1.0% for pastel shades and 1.0–2.5% for vivid shades.
Which pigments are suitable for PET?
Since PET's typical melt temperature is 260–280 °C, pigments with a heat resistance above this range should be selected. Titanium dioxide, carbon black and iron oxide red have a heat resistance above 300 °C and phthalocyanine blue and green 280–300 °C; diarylide yellow and orange, with a heat resistance of 200–230 °C, are not suitable for these temperatures.